Yes, I did have them mixed up.  We have PLA, not ABS.  Geordie
straightened me out by showing me printed samples of both.

On 29 November 2011 10:25, Kevin Martin <kpmartin at thinkage.ca> wrote:
> Doug,
> Do you have PLA and ABS mixed up in part of this?
> "The usual recommended temperature for PLA is 190 C, but we have been
> printing at higher temperatures than this, which makes drooling worse.
> So we should try lower termperatures."
> As far as I know we have never extruded PLA.
>
> -Kevin Martin